Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Casting steel

Characteristics for grade     16KH18N12S4TYUL   ( 16Х18Н12С4ТЮЛ )



      Grade :     16KH18N12S4TYUL   ( 16Х18Н12С4ТЮЛ )
      Classification :   Casting alloy steel with specific properties
      Equivalent grades:     Is absent



Chemical composition in % for grade   16KH18N12S4TYUL   ( 16Х18Н12С4ТЮЛ )
C Si Mn Ni S P Cr TiAl
0.13 - 0.193.8 - 4.50.5 - 111 - 13max   0.03max   0.0317 - 190.4 - 0.70.13 - 0.35


Mechanical properties under Т=20oС for grade   16KH18N12S4TYUL   ( 16Х18Н12С4ТЮЛ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 977-88     491 245 15 30275Guenching 1150 - 1200oC,Cooling water,


Heat treatment of the material   16KH18N12S4TYUL   ( 16Х18Н12С4ТЮЛ )
Hardening 1150 - 1200 ° C, Air cooling



Types of delivery of grade   16KH18N12S4TYUL   ( 16Х18Н12С4ТЮЛ )
B82 - Steel Castings


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  16KH18N12S4TYUL   ( 16Х18Н12С4ТЮЛ ) - Casting alloy steel with specific properties: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru