Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Casting steel

Characteristics for grade     07KH18N9L   ( 07Х18Н9Л )



      Grade :     07KH18N9L   ( 07Х18Н9Л )
      Classification :   Casting alloy steel with specific properties
      Equivalent grades:   Go here



Chemical composition in % for grade   07KH18N9L   ( 07Х18Н9Л )
C Si Mn Ni S P Cr Cu
max   0.070.2 - 11 - 28 - 11max   0.03max   0.03517 - 20max   0.3


Mechanical properties under Т=20oС for grade   07KH18N9L   ( 07Х18Н9Л )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting     450 180 25 351000Guenching 1050 - 1100oC,Cooling air,


Equivalent steels for grade     07KH18N9L   ( 07Х18Н9Л )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandItalySwedenCzechia
-DIN,WNrJIS AFNORBSUNISSCSN
CF-8
J92730
1.4308
G-X12CrNi18-11
G-X6CrNi18-9
G-X8CrNi18-10
GX5CrNi19-10
SCS13
Z6CN18-10M
Z6CN18.1OM
304C15
GX6CrNi20-10
2333
422930




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  07KH18N9L   ( 07Х18Н9Л ) - Casting alloy steel with specific properties: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys