Characteristics for grade     10KH18N11BL   ( 10Х18Н11БЛ )



      Grade :     10KH18N11BL   ( 10Х18Н11БЛ )
      Classification :   Casting alloy steel with specific properties
      Equivalent grades:   Go here



Chemical composition in % for grade   10KH18N11BL   ( 10Х18Н11БЛ )
C Si Mn Ni S P Cr Nb
max   0.10.2 - 11 - 28 - 12max   0.03max   0.03517 - 200.45 - 0.9


Mechanical properties under Т=20oС for grade   10KH18N11BL   ( 10Х18Н11БЛ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 977-88     441 196 25 35590Guenching 1100 - 1150oC,Cooling water,


Heat treatment of the material   10KH18N11BL   ( 10Х18Н11БЛ )
Hardening 1100 - 1150 ° C, Water cooling


Equivalent steels for grade     10KH18N11BL   ( 10Х18Н11БЛ )
Warning! Indicated both exact and nearest equivalents.
USAGermany
-DIN,WNr
J92640
GX5CrNiNb19-11



Types of delivery of grade   10KH18N11BL   ( 10Х18Н11БЛ )
B82 - Steel Castings


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  10KH18N11BL   ( 10Х18Н11БЛ ) - Casting alloy steel with specific properties: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru