Grade : | 20KH17N2 ( 20Х17Н2 ) ( 2Х17Н2 ) |
Classification : | Corrosion-resistant steel for general purposes |
Equivalent grades: | Go here |
C | Si | Mn | Ni | S | P | Cr |
0.17 - 0.25 | max 0.8 | max 0.8 | 1.5 - 2.5 | max 0.025 | max 0.035 | 16 - 18 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Forging, GOST 25054-81 | to 600 | longitudinal | 813 | 666 | 12-15 | 30-40 | 490-590 | Guenching and drawing |
Brinell hardness for 20KH17N2 ( 20Х17Н2 ) (annealing) , Bar GOST 5949-75 | HB 10 -1 = 285 MPa |
Brinell hardness for 20KH17N2 ( 20Х17Н2 ) , Forging GOST 25054-81 | HB 10 -1 = 248 - 293 MPa |
USA | Germany | Japan | France | England | European | Italy | Spain | China | Sweden | |||||||||||||||||
- | DIN,WNr | JIS | AFNOR | BS | EN | UNI | UNE | GB | SS | |||||||||||||||||
|
|
|
|
|
|
|
|
|
|
B03 - Metal forming treatment. Forgings |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |