Characteristics for grade     R6M5F3   ( Р6М5Ф3 )



      Grade :     R6M5F3   ( Р6М5Ф3 )
      Classification :   High speed tool steel
      Equivalent grades:   Go here



Chemical composition in % for grade   R6M5F3   ( Р6М5Ф3 )
C Si Mn Ni S P Cr Mo W V Co Cu
0.95 - 1.050.2 - 0.50.2 - 0.5max   0.6max   0.025max   0.033.8 - 4.34.8 - 5.35.7 - 6.72.3 - 2.7max   0.5max   0.25


Temperature of critical points for grade   R6M5F3   ( Р6М5Ф3 ).
Ac1 = 815


    Brinell hardness for     R6M5F3   ( Р6М5Ф3 )   (annealing) ,       GOST 19265-73 HB 10 -1 = 269   MPa


Equivalent steels for grade     R6M5F3   ( Р6М5Ф3 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapan
-DIN,WNrJIS
T11313
T11323
S6-5-3
SKH52
SKH53



Types of delivery of grade   R6M5F3   ( Р6М5Ф3 )
В22 - Graded and shaped rolling
В32 - Graded and shaped rolling
B33 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  R6M5F3   ( Р6М5Ф3 ) - High speed tool steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru