Characteristics for grade     20GL   ( 20ГЛ )



      Grade :     20GL   ( 20ГЛ )
      Classification :   Casting alloy steel for general purposes
      Equivalent grades:   Go here



Chemical composition in % for grade   20GL   ( 20ГЛ )
C Si Mn S P
0.15 - 0.250.2 - 0.41.2 - 1.6max   0.04max   0.04


Mechanical properties under Т=20oС for grade   20GL   ( 20ГЛ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 977-88     540 275 18 25491 
Casting, GOST 977-88     530 334 14 25383 
Casting, GOST 21357-87     500 300 20 35 Normalizing
Casting, GOST 21357-87     550 400 15 30 Guenching and drawing


    Brinell hardness for     20GL   ( 20ГЛ )   ,       HB 10 -1 = 143 - 187   MPa


Heat treatment of the material   20GL   ( 20ГЛ )
Normalizing 880 - 900 ° C, Tempering 600 - 650 ° C
Hardening 870 - 890 ° C, Tempering 620 - 650 ° C


Equivalent steels for grade     20GL   ( 20ГЛ )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanEuropeanItalyBulgariaHungaryPolandRomaniaCzechiaAustria
-DIN,WNrJIS EN UNIBDSMSZPNSTASCSNONORM
A352GrLCC
GrA2Q
GrWCC
J02503
J02505
1.1120
1.1133
G17Mn5
GS20Mn5
SCA1
SCMn1
G21Mn5
G22Mn3
20L
Ao20Mn6
L20G
T20Mn14
422714
GS21Mn5



Types of delivery of grade   20GL   ( 20ГЛ )
B42 - Rails: Pads, Pads, Crutches
B82 - Steel Castings
B83 - Castings with special properties (cast iron and steel)


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  20GL   ( 20ГЛ ) - Casting alloy steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru