Characteristics for grade     12DKHN1MFL   ( 12ДХН1МФЛ )



      Grade :     12DKHN1MFL   ( 12ДХН1МФЛ )
      Classification :   Casting alloy steel for general purposes
      Equivalent grades:   Go here



Chemical composition in % for grade   12DKHN1MFL   ( 12ДХН1МФЛ )
C Si Mn Ni S P Cr Mo V Cu
0.1 - 0.180.2 - 0.40.3 - 0.551.4 - 1.8max   0.03max   0.031.2 - 1.70.2 - 0.30.08 - 0.150.4 - 0.65


Mechanical properties under Т=20oС for grade   12DKHN1MFL   ( 12ДХН1МФЛ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 977-88     785 638 12 20294 
Casting, GOST 977-88     981 735 10 20294 


    Brinell hardness for     12DKHN1MFL   ( 12ДХН1МФЛ )   ,       HB 10 -1 = 217 - 269   MPa


Heat treatment of the material   12DKHN1MFL   ( 12ДХН1МФЛ )
Normalizing 940 - 960 ° C, or Normalizing 890 - 910 ° C, Tempering 520 - 630 ° C
Hardening 890 - 910 ° C, Tempering 520 - 630 ° C


Equivalent steels for grade     12DKHN1MFL   ( 12ДХН1МФЛ )
Warning! Indicated both exact and nearest equivalents.
BulgariaRomania
BDSSTAS
12DChNMFL
T14VMoCuCrNi16



Types of delivery of grade   12DKHN1MFL   ( 12ДХН1МФЛ )
B82 - Steel Castings


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  12DKHN1MFL   ( 12ДХН1МФЛ ) - Casting alloy steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru