Chemical composition in % for grade   23KHGS2MFL   ( 23ХГС2МФЛ )
C Si Mn S P Cr Mo V
0.18 - 0.241.8 - 20.5 - 0.8max   0.025max   0.0250.6 - 0.90.25 - 0.30.1 - 0.15


Mechanical properties under Т=20oС for grade   23KHGS2MFL   ( 23ХГС2МФЛ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 977-88     1275 1079 6 24392Guenching 980 - 1000oC,Drawing 200 - 230oC,


Heat treatment of the material   23KHGS2MFL   ( 23ХГС2МФЛ )
Pre - processing - Normalizing 1000 - 1040 ° C, Tempering 720 - 740 ° C
Final processing - Hardening 1000 - 1020 ° C, Tempering 180 - 220 ° C



Types of delivery of grade   23KHGS2MFL   ( 23ХГС2МФЛ )
B82 - Steel Castings


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  23KHGS2MFL   ( 23ХГС2МФЛ ) - Casting alloy steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru