Grade : | 08KH14NDL ( 08Х14НДЛ ) |
Classification : | Casting alloy steel with specific properties |
Equivalent grades: | Go here |
C | Si | Mn | Ni | S | P | Cr | Cu |
max 0.08 | max 0.4 | 0.5 - 0.8 | 1.2 - 1.6 | max 0.025 | max 0.025 | 13 - 14.5 | 0.8 - 1.2 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Casting, GOST 977-88 | 648 | 510 | 15 | 40 | 590 |
Hardening 1000 - 1200 ° C, Air cooling; Tempering 660 - 700 ° C , Air cooling; |
USA | |
- | |
|
B82 - Steel Castings |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |