Characteristics for grade     08KH15N4DML   ( 08Х15Н4ДМЛ )



      Grade :     08KH15N4DML   ( 08Х15Н4ДМЛ )
      Classification :   Casting alloy steel with specific properties
      Equivalent grades:   Go here



Chemical composition in % for grade   08KH15N4DML   ( 08Х15Н4ДМЛ )
C Si Mn Ni S P Cr Mo Cu
max   0.08max   0.41 - 1.53.5 - 3.9max   0.025max   0.02514 - 160.3 - 0.451 - 1.4


Mechanical properties under Т=20oС for grade   08KH15N4DML   ( 08Х15Н4ДМЛ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 977-88     736 589 17 45981 


Heat treatment of the material   08KH15N4DML   ( 08Х15Н4ДМЛ )
Hardening 1030 - 1050 ° C, Air cooling; Tempering 600 - 620 ° C , Air cooling


Equivalent steels for grade     08KH15N4DML   ( 08Х15Н4ДМЛ )
Warning! Indicated both exact and nearest equivalents.
USAGermany
-DIN,WNr
J92180
GX4CrNiCuNb16-4



Types of delivery of grade   08KH15N4DML   ( 08Х15Н4ДМЛ )
B82 - Steel Castings


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  08KH15N4DML   ( 08Х15Н4ДМЛ ) - Casting alloy steel with specific properties: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru