Characteristics for grade     15KH18N22V6M2RL   ( 15Х18Н22В6М2РЛ )



      Grade :     15KH18N22V6M2RL   ( 15Х18Н22В6М2РЛ )
      Classification :   Casting alloy steel with specific properties
      Equivalent grades:     Is absent



Chemical composition in % for grade   15KH18N22V6M2RL   ( 15Х18Н22В6М2РЛ )
Fe C Si Mn Ni S P Cr Mo W B
46.525 - 56.40.1 - 0.20.2 - 0.60.3 - 0.620 - 24max   0.03max   0.03516 - 182 - 35 - 7max   0.01


Mechanical properties under Т=20oС for grade   15KH18N22V6M2RL   ( 15Х18Н22В6М2РЛ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 977-88     491 196 5    


Heat treatment of the material   15KH18N22V6M2RL   ( 15Х18Н22В6М2РЛ )
Aging 790 - 810 ° C, 12 - 16 hours , Air cooling



Types of delivery of grade   15KH18N22V6M2RL   ( 15Х18Н22В6М2РЛ )
B82 - Steel Castings


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  15KH18N22V6M2RL   ( 15Х18Н22В6М2РЛ ) - Casting alloy steel with specific properties: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru