Characteristics for grade     9KHF   ( 9ХФ )



      Grade :     9KHF   ( 9ХФ )
      Classification :   Alloy tool steel
      Equivalent grades:   Go here



Chemical composition in % for grade   9KHF   ( 9ХФ )
C Si Mn Ni S P Cr V Cu
0.8 - 0.90.1 - 0.40.3 - 0.6max   0.4max   0.03max   0.030.4 - 0.70.15 - 0.3max   0.3


Temperature of critical points for grade   9KHF   ( 9ХФ ).
Ac1 = 700 ,       Mn = 215


Mechanical properties under Т=20oС for grade   9KHF   ( 9ХФ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Band annealed , GOST 2283-79 0.1 - 4   930        


    Brinell hardness for     9KHF   ( 9ХФ )   (heat treatment) ,       GOST 5950-2000 HB 10 -1 = 241   MPa


Equivalent steels for grade     9KHF   ( 9ХФ )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanBulgariaPolandCzechiaAustria
-DIN,WNrJIS BDSPNCSNONORM
L2
1.1056
1.2056
80CrV2
90Cr3
SKC11
8ChF
NCV1
19419
19423
BOHLERB400



Types of delivery of grade   9KHF   ( 9ХФ )
В32 - Graded and shaped rolling
B34 - Ribbons


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  9KHF   ( 9ХФ ) - Alloy tool steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru