Characteristics for grade     8KH4V2MFS2   ( 8Х4В2МФС2 )



      Grade :   8KH4V2MFS2   ( 8Х4В2МФС2 ) (   ЭП761   )
      Classification :   Alloy tool steel
      Equivalent grades:     Is absent



Chemical composition in % for grade   8KH4V2MFS2   ( 8Х4В2МФС2 )
C Si Mn Ni S P Cr Mo W V Cu
0.8 - 0.91.7 - 20.2 - 0.5max   0.4max   0.03max   0.034.5 - 5.10.8 - 1.11.8 - 2.31.1 - 1.4max   0.3


Temperature of critical points for grade   8KH4V2MFS2   ( 8Х4В2МФС2 ).
Ac1 = 840 ,      Ac3(Acm) = 880 ,       Ar1 = 785 ,       Mn = 150


Mechanical properties under Т=20oС for grade   8KH4V2MFS2   ( 8Х4В2МФС2 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
        2700-2800    Guenching and drawing


    Brinell hardness for     8KH4V2MFS2   ( 8Х4В2МФС2 )   (annealing) ,       GOST 5950-2000 HB 10 -1 = 255   MPa



Types of delivery of grade   8KH4V2MFS2   ( 8Х4В2МФС2 )
В32 - Graded and shaped rolling


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  8KH4V2MFS2   ( 8Х4В2МФС2 ) - Alloy tool steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru