Grade : | 4KH2V5MF ( 4Х2В5МФ ) ( ЭИ959 ) |
Classification : | Die tool steel |
Equivalent grades: | Go here |
C | Si | Mn | Ni | S | P | Cr | Mo | W | V | Cu |
0.3 - 0.4 | 0.1 - 0.4 | 0.1 - 0.45 | max 0.4 | max 0.03 | max 0.03 | 2.2 - 3 | 0.6 - 0.9 | 4.5 - 5.5 | 0.6 - 0.9 | max 0.3 |
Ac1 = 820 , Ac3(Acm) = 940 , Ar3(Arcm) = 840 , Ar1 = 690 , Mn = 205 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Blank | 15 | 1680 | 1480 | 10 | 42 | 300 | Guenching 1080oC, oil, |
Brinell hardness for 4KH2V5MF ( 4Х2В5МФ ) (annealing) , GOST 5950-2000 | HB 10 -1 = 241 MPa |
Germany | Japan | France | Italy | Poland | Czechia | Austria | |||||||
DIN,WNr | JIS | AFNOR | UNI | PN | CSN | ONORM | |||||||
|
|
|
|
|
|
|
В32 - Graded and shaped rolling |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2025 Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use. |