Characteristics for grade     27KKH   ( 27КХ )



      Grade :     27KKH   ( 27КХ )
      Classification :   Magnetically soft precision alloy
      Equivalent grades:     Is absent



Chemical composition in % for grade   27KKH   ( 27КХ )
C Si Mn Ni S P Cr Co
max   0.04max   0.250.2 - 0.4max   0.3max   0.015max   0.0150.3 - 0.626.5 - 28


Mechanical properties under Т=20oС for grade   27KKH   ( 27КХ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Band, GOST 10160-75     590 295 20    
Band cold-worked , GOST 10160-75     1080   2    


Physical properties for grade   27KKH   ( 27КХ )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.2     7980   200
100   10.7        



Types of delivery of grade   27KKH   ( 27КХ )
В30 - Classification, nomenclature and general norms


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  27KKH   ( 27КХ ) - Magnetically soft precision alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys