Characteristics for grade     KhN70Yu   ( ХН70Ю )

      Grade :   KhN70Yu   ( ХН70Ю ) (   ЭИ652   )
      Classification :   Hidh-temperature or heat-resistant alloy
      Equivalent grades:   Go here



Chemical composition in % for grade   KhN70Yu   ( ХН70Ю )
Fe C Si Mn Ni S P Cr CeAl Cu Ba
max   1max   0.1max   0.8max   0.365.073 - 71.2max   0.012max   0.01526 - 29max   0.032.8 - 3.5max   0.07max   0.1


Mechanical properties under Т=20oС for grade   KhN70Yu   ( ХН70Ю )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet, GOST 24982-81 to 3.9   980   30   Guenching 1100 - 1150oC,Cooling water,


Technological properties for grade   KhN70Yu   ( ХН70Ю )
  Weldability: limited weldability.


Physical properties for grade   KhN70Yu   ( ХН70Ю )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.91   11.7 7900    
100 1.82 13.14 12.6      
200 1.73 13.86 13.9      
300 1.66 14.76 13.55      
400 1.56 15.68 17.25      
500 1.47 16.39 18.9      
600 1.37 17.81 18.9      
700 1.18 22.42 23.1      
800   25.47 24.8      
900   21.34 26.9      
1000   21.21        
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     KhN70Yu   ( ХН70Ю )
Warning! Indicated both exact and nearest equivalents.
Germany
DIN,WNr
2.4872
NiCr20AlSi


Assortment for grade   KhN70Yu   ( ХН70Ю )
B23 - Sheets and Strips
  GOST   19903 - 74 Hot-rolled steel sheets
  GOST   19904 - 90 Cold-rolled steel sheets
B33 - Sheets and Strips
  GOST   24982 - 81 Rolled sheet of corrosion-resistant, heatresistant and heat-proof alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  KhN70Yu   ( ХН70Ю ) - Hidh-temperature or heat-resistant alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru