Grade : | 36NKHTYU5M ( 36НХТЮ5М ) |
Classification : | Precision alloy for elastic elements |
Equivalent grades: | Is absent |
Fe | C | Si | Mn | Ni | S | P | Cr | Mo | Ti | Al |
37.01 - 43.7 | max 0.05 | 0.3 - 0.7 | 0.8 - 1.2 | 35 - 37 | max 0.02 | max 0.02 | 12.5 - 13.5 | 4 - 6 | 2.7 - 3.2 | 1 - 1.3 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Bar, GOST 14119-85 | 1030 | 635 | 10 | 20 | 290 | Hardening and ageing | ||
Wire, GOST 10994-74 | 1375-1765 | |||||||
Band cold-worked , GOST 14117-85 | 1100 | 1 | ||||||
Band, GOST 14117-85 | 880-930 | 15-20 | Guenching |
Brinell hardness for 36NKHTYU5M ( 36НХТЮ5М ) , | HB 10 -1 = 400 - 420 MPa |
В22 - Graded and shaped rolling |
В32 - Graded and shaped rolling |
B34 - Ribbons |
B73 - Steel Alloy Wire |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |