Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | 20KH13N4G9 ( 20Х13Н4Г9 ) ( 2Х13Н4Г9 ЭИ100 ) |
Classification : | Corrosion-resistant steel for general purposes |
Equivalent grades: | Is absent |
C | Si | Mn | Ni | S | P | Cr |
0.15 - 0.3 | max 0.8 | 8 - 10 | 3.7 - 4.7 | max 0.025 | max 0.05 | 12 - 14 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Bar, GOST 5949-75 | 640 | 245 | 35 | 55 | Guenching | |||
Sheet thin, GOST 4986-79 | 590 | 18-35 | Guenching 1050 - 1080oC,Cooling air, | |||||
Sheet thin cold-worked , GOST 5582-75 | 980 | 15 | ||||||
Sheet thin, GOST 5582-75 | 640 | 40 | Guenching 1050 - 1080oC,Cooling water, |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
B34 - Ribbons |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |