Characteristics for grade     07KH16N6   ( 07Х16Н6 )



      Grade :   07KH16N6   ( 07Х16Н6 ) (   Х16Н6     ЭП288   )
      Classification :   Corrosion-resistant steel for general purposes
      Equivalent grades:   Go here



Chemical composition in % for grade   07KH16N6   ( 07Х16Н6 )
C Si Mn Ni S P Cr
0.05 - 0.09max   0.8max   0.85 - 8max   0.02max   0.03515.5 - 17.5


Mechanical properties under Т=20oС for grade   07KH16N6   ( 07Х16Н6 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 5949-75     1080 880 12 50690 
Forging, GOST 25054-81     1176 980 12-1350690 
Sheet trick, GOST 7350-77     1180 390 15   Normalizing 1030 - 1050oC, air,
Sheet thin, GOST 5582-75     1180   20   Guenching 1030 - 1070oC,Cooling water,


    Brinell hardness for     07KH16N6   ( 07Х16Н6 )   ,     Forging GOST 25054-81 HB 10 -1 = 341 - 415   MPa


Equivalent steels for grade     07KH16N6   ( 07Х16Н6 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandItalySweden
-DIN,WNrJIS AFNORBSUNISS
301
S30100
1.4310
X10CrNi18-8
X12CrNi17-7
SUS301
Z11CN17-08
301S21
301S22
CrNi17/7
X10CrNi18-8
X12CrNi17-07
2331



Types of delivery of grade   07KH16N6   ( 07Х16Н6 )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  07KH16N6   ( 07Х16Н6 ) - Corrosion-resistant steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru