Grade : | 15KH18N12S4TYU ( 15Х18Н12С4ТЮ ) ( ЭИ654 ) |
Classification : | Corrosion-resistant steel for general purposes |
Equivalent grades: | Is absent |
C | Si | Mn | Ni | S | P | Cr | Ti | Al |
0.12 - 0.17 | 3.8 - 4.5 | 0.5 - 1 | 11 - 13 | max 0.03 | max 0.035 | 17 - 19 | 0.4 - 0.7 | 0.13 - 0.35 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Bar, GOST 5949-75 | Ø 60 | 720 | 375 | 25 | 40 | 780 | Guenching 950 - 1050oC,Cooling water, | |
Forging, GOST 25054-81 | to 600 | longitudinal | 715 | 382 | ||||
Sheet trick, GOST 7350-77 | 690-930 | 345 | 30 | Guenching 1020 - 1050oC,Cooling water, | ||||
Sheet thin, GOST 5582-75 | 720 | 345 | 30 | Guenching 1020 - 1050oC, water, | ||||
Sheet thin cold-worked , GOST 5582-75 | 880 | 685 | 10 | |||||
Sheet thin, GOST 4986-79 | 690 | 13-25 | Guenching 1020 - 1050oC,Cooling water, | |||||
Sheet thin cold-worked , GOST 4986-79 | 830-1080 | 5-10 |
B03 - Metal forming treatment. Forgings |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
B34 - Ribbons |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2025 Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use. |