Characteristics for grade     03KH17N14M3   ( 03Х17Н14М3 )

      Grade :   03KH17N14M3   ( 03Х17Н14М3 ) (   000Х17Н13М2   )
      Classification :   Сryogenic structural steel
      Equivalent grades:   Go here



Chemical composition in % for grade   03KH17N14M3   ( 03Х17Н14М3 )
C Si Mn Ni S P Cr Mo
max   0.03max   0.41 - 213 - 15max   0.02max   0.03516 - 182.5 - 3.1


Mechanical properties under Т=20oС for grade   03KH17N14M3   ( 03Х17Н14М3 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 5949-75 Ø 60   490 196 40   Guenching 1070 - 1100oC,Cooling water,
Forging, GOST 25054-81     470 176 35-4045-55  
Sheet trick, GOST 7350-77     490 196 40   Guenching 1080 - 1100oC,Cooling water,
Sheet thin, GOST 5582-75     490 196 40   Guenching 1030 - 1070oC, air,


    Brinell hardness for     03KH17N14M3   ( 03Х17Н14М3 )   ,     Forging GOST 25054-81 HB 10 -1 = 179   MPa


Technological properties for grade   03KH17N14M3   ( 03Х17Н14М3 )
  Weldability: without limitations.


Physical properties for grade   03KH17N14M3   ( 03Х17Н14М3 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       8000    


Equivalent steels for grade     03KH17N14M3   ( 03Х17Н14М3 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySpainChinaSwedenBulgariaHungaryRomaniaCzechiaFinlandAustriaAustraliaSouth Korea
-DIN,WNrJIS AFNORBSEN UNIUNEGBSSBDSMSZSTASCSNSFSONORMASKS
316
316L
S31600
S31603
S31673
S31683
1.4404
1.4435
1.4436
X2CrNiMo17-12-2
X2CrNiMo17-12-3
X2CrNiMo18-12
X2CrNiMo18-14-3
X3CrNiMo17-13-3
SCS16
SUS316L
X2CrNiMo18-14-3
X2CrNiMo18-15-4
Z2CND17-12
Z3CND17-11-02
Z3CND17-12-03
Z3CND18-14-03
Z3CND18-14-08
Z3CND19-15-04
Z6CND18-12-03
316L
316S11
316S13
316S14
316S31
316S33
LW22
LWCF22
X2CrNiMo17-12-3
X2CrNiMo18-14-3
1.4432
1.4435
X2CrNiMo17-12-3
X2CrNiMo18-14-3
316LM1
X2CrNiMo17-13
X2CrNiMo17-13KG
X2CrNiMo18-14-3
F.3533
X2CrNiMo17132
00Cr17Ni14Mo2
00Cr17Ni14Mo3
2343
2353
X2CrNiMo18-14-3
KO38LC
X2CrNiMo18-14-3
2MoNiCr175
17350
X2CrNiMo17-13-3
X2CrNiMo18-14-3KW
316L
STS316L
STSF316L

Types of delivery of grade   03KH17N14M3   ( 03Х17Н14М3 )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
В62 - Steel pipes and connecting parts to them


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  03KH17N14M3   ( 03Х17Н14М3 ) - Сryogenic structural steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru