Characteristics for grade     04KH18N10   ( 04Х18Н10 )



      Grade :   04KH18N10   ( 04Х18Н10 ) (   00Х18Н10     ЭИ842     ЭП550   )
      Classification :   Corrosion-resistant steel for general purposes
      Equivalent grades:   Go here



Chemical composition in % for grade   04KH18N10   ( 04Х18Н10 )
C Si Mn Ni S P Cr
max   0.04max   0.8max   29 - 11max   0.02max   0.03517 - 19


Mechanical properties under Т=20oС for grade   04KH18N10   ( 04Х18Н10 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe cooling strain, GOST 9941-81     490   45    
Pipe hot strain, GOST 9940-81     441   40    
Bar, GOST 5949-75     440 155 40 55 Guenching 1020 - 1100oC, air,
Forging, GOST 25054-81     441 157 38-4045-50  
Sheet trick, GOST 7350-77     490 175 45   Guenching 1050 - 1100oC,Cooling water,


    Brinell hardness for     04KH18N10   ( 04Х18Н10 )   ,     Forging GOST 25054-81 HB 10 -1 = 179   MPa


Physical properties for grade   04KH18N10   ( 04Х18Н10 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       7900    


Equivalent steels for grade     04KH18N10   ( 04Х18Н10 )
Warning! Indicated both exact and nearest equivalents.
USAJapanFranceEnglandEuropeanSweden
-JIS AFNORBSEN SS
304L
SUS304L
Z3CN18–10
304S11
1.4307
X2CrNi18-9
2352



Types of delivery of grade   04KH18N10   ( 04Х18Н10 )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
В62 - Steel pipes and connecting parts to them


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  04KH18N10   ( 04Х18Н10 ) - Corrosion-resistant steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys