Grade : | 12KH18N10E ( 12Х18Н10Е ) ( X18H10E ЭП47 ) |
Classification : | Corrosion-resistant steel for general purposes |
Equivalent grades: | Go here |
C | Si | Mn | Ni | S | P | Cr | Se |
max 0.12 | max 0.8 | max 2 | 9 - 11 | max 0.02 | max 0.035 | 17 - 19 | 0.18 - 0.35 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Sheet thin, GOST 5582-75 | 740 | 35 | Guenching 1050 - 1080oC, air, | |||||
Sheet thin, GOST 4986-79 | 740 | 18-35 | Guenching 1050 - 1080oC, air, |
USA | Japan | England | |||
- | JIS | BS | |||
|
|
|
B23 - Sheets and Strips |
B33 - Sheets and Strips |
B34 - Ribbons |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |