Characteristics for grade     03KH18N11   ( 03Х18Н11 )

      Grade :   03KH18N11   ( 03Х18Н11 ) (   000Х18Н11   )
      Classification :   Corrosion-resistant steel for general purposes
      Equivalent grades:   Go here
Grade   03KH18N11   ( 03Х18Н11 ):   supplier   Auremo   www.auremo.biz
Sale:   Russia +7 (812) 680-16-77 ,   Germany +49 (208) 376-298-00 ,     info [a] auremo.org



Chemical composition in % for grade   03KH18N11   ( 03Х18Н11 )
C Si Mn Ni S P Cr
max   0.03max   0.8max   210.5 - 12.5max   0.02max   0.03517 - 19


Mechanical properties under Т=20oС for grade   03KH18N11   ( 03Х18Н11 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 5949-75 to Ø 60   440 155 40 55 Guenching 1020 - 1100oC,Cooling air,
Forging, GOST 25054-81     441 176 40 45-55  
Sheet trick, GOST 7350-77     490 196 40   Guenching
Sheet thin, GOST 5582-75     490 196 40   Guenching 1050 - 1080oC,Cooling water,


    Brinell hardness for     03KH18N11   ( 03Х18Н11 )   ,     Forging GOST 25054-81 HB 10 -1 = 179   MPa


Equivalent steels for grade     03KH18N11   ( 03Х18Н11 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySpainChinaSwedenPolandCzechiaFinlandAustria
-DIN,WNrJIS AFNORBSEN UNIUNEGBSSPNCSNSFSONORM
304L
304LN
S30403
1.4306
1.4311
GX2CrNi19-11
X2CrNi18-9
X2CrNi19-11
X2CrNiN18-10
SCS19
SUS304
SUS304L
304F10
Z1CN18-12
Z2CN18-09
Z2CN1810
Z3CN18-10
Z3CN18-11
Z3CN19-10M
Z3CN19-11
304C12
304S11
304S12
304S62
LW20
LWCF20
1.4306
X2CrNi10
X2CrNi18-10
X2CrNi19-11
X2CrNi18-11
X3CrNi18-11
F.3503
X2CrNi1810
00Cr19Ni10
00Cr19Ni11
2333
2352
00H18N10
17249
720
X2CrNi19-11KKW

Types of delivery of grade   03KH18N11   ( 03Х18Н11 )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  03KH18N11   ( 03Х18Н11 ) - Corrosion-resistant steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru