Grade : | 08KH18N12T ( 08Х18Н12Т ) ( 0Х18Н12Т ) |
Classification : | Corrosion-resistant steel for general purposes |
Equivalent grades: | Go here |
C | Si | Mn | Ni | S | P | Cr | - |
max 0.08 | max 0.8 | max 2 | 11 - 13 | max 0.02 | max 0.035 | 17 - 19 | 5(С - 0.6) Ti, остальное Fe |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Pipe cooling strain, GOST 9941-81 | 549 | 37 | ||||||
Pipe hot strain, GOST 9940-81 | 510 | 40 | ||||||
Sheet trick, GOST 7350-77 | 510 | 205 | 43 | Guenching 1030 - 1080oC,Cooling air, | ||||
Sheet thin, GOST 5582-75 | 510 | 35 | Guenching 1050 - 1080oC,Cooling water, |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 7950 |
USA | Germany | European | ||||
- | DIN,WNr | EN | ||||
|
|
|
B23 - Sheets and Strips |
B33 - Sheets and Strips |
В62 - Steel pipes and connecting parts to them |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2025 Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use. |