Characteristics for grade     KhN38VT   ( ХН38ВТ )

      Grade :   KhN38VT   ( ХН38ВТ ) (   ЭИ703   )
      Classification :   Hidh-temperature or heat-resistant alloy
      Equivalent grades:   Go here



Chemical composition in % for grade   KhN38VT   ( ХН38ВТ )
Fe C Si Mn Ni S P Cr Ce W TiAl
31.08 - 41.440.06 - 0.12max   0.8max   0.735 - 39max   0.02max   0.0320 - 23max   0.052.8 - 3.50.7 - 1.2max   0.5


Mechanical properties under Т=20oС for grade   KhN38VT   ( ХН38ВТ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet, GOST 24982-81     800-830  35   Guenching


Equivalent steels for grade     KhN38VT   ( ХН38ВТ )
Warning! Indicated both exact and nearest equivalents.
USAGermany
-DIN,WNr
N08825
NiCr21Mo


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

  KhN38VT   ( ХН38ВТ ) - Hidh-temperature or heat-resistant alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru