Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | KHN65MV ( ХН65МВ ) ( 0Х15Н65М16В ЭП567 ) |
Classification : | Corrosion-resistant alloy |
Equivalent grades: | Go here |
Fe | C | Si | Mn | Ni | S | P | Cr | Mo | W |
max 1 | max 0.03 | max 0.15 | max 1 | 59.793 - 67.5 | max 0.012 | max 0.015 | 14.5 - 16.5 | 15 - 17 | 3 - 4.5 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Sheet, GOST 24982-81 | 830-850 | 390-410 | 40 | Guenching 1050 - 1090oC, | ||||
Forging, GOST 25054-81 | 735 | 294 | 30-35 | 35-40 |
Brinell hardness for KHN65MV ( ХН65МВ ) , Forging GOST 25054-81 | HB 10 -1 = 220 MPa |
USA | Germany | ||||||
- | DIN,WNr | ||||||
|
|
B03 - Metal forming treatment. Forgings |
B23 - Sheets and Strips |
B33 - Sheets and Strips |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2025 Database of Steel and Alloy (russian title is the Marochnik)