Chemical composition in % for grade   KH15YU5   ( Х15Ю5 )
C Si Mn Ni S P Cr Ce TiAl Ca -
max   0.08max   0.7max   0.7max   0.6max   0.015max   0.0313.5 - 15.5max   0.10.2 - 0.64.5 - 5.5max   0.1 Са, Ce - расчет


Mechanical properties under Т=20oС for grade   KH15YU5   ( Х15Ю5 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Wire, GOST 12766.1-90     740   16    
Band, GOST 12766.2-90     736   16    


    Brinell hardness for     KH15YU5   ( Х15Ю5 )   ,       GOST 12766.1-90 HB 10 -1 = 150 - 200   MPa


Technological properties of the material   KH15YU5   ( Х15Ю5 ) .
        Melting temperature : 1500   °C


Physical properties for grade   KH15YU5   ( Х15Ю5 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       7280   1290
100   16     480  



Types of delivery of grade   KH15YU5   ( Х15Ю5 )
В32 - Graded and shaped rolling
B34 - Ribbons
B73 - Steel Alloy Wire


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  KH15YU5   ( Х15Ю5 ) - Precision alloy with higt electric resistance: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru