Grade : | KH15N60 ( Х15Н60 ) |
Classification : | Precision alloy with higt electric resistance |
Equivalent grades: | Is absent |
Fe | C | Si | Mn | Ni | S | P | Cr | Ti | Al |
17.3 - 29.2 | max 0.15 | 0.8 - 1.5 | max 1.5 | 55 - 61 | max 0.02 | max 0.03 | 15 - 18 | max 0.3 | max 0.2 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Wire, GOST 8803-89 | 600-660 | |||||||
Band, GOST 12766.2-90 | 834 | 20 |
Brinell hardness for KH15N60 ( Х15Н60 ) , GOST 12766.1-90 | HB 10 -1 = 140 - 150 MPa |
Melting temperature : | 1390 °C |
Forging temperature : | 1100 - 1000 °C |
Annealing temperature : | 750 - 850 °C |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 2.18 | 8200 | 1100 | |||
100 | 17 | 460 |
B34 - Ribbons |
B73 - Steel Alloy Wire |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2025 Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use. |