Characteristics for grade     KH20N80-VI   ( Х20Н80-ВИ )



      Grade :     KH20N80-VI   ( Х20Н80-ВИ )
      Classification :   Precision alloy with higt electric resistance
      Equivalent grades:     Is absent



Chemical composition in % for grade   KH20N80-VI   ( Х20Н80-ВИ )
Fe C Si Mn Ni S P Cr TiAl
max   1.5max   0.050.4 - 1max   0.373.93 - 79.585max   0.01max   0.0120 - 23max   0.050.015 - 0.15


Mechanical properties under Т=20oС for grade   KH20N80-VI   ( Х20Н80-ВИ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Wire, GOST 8803-89     620-680       


Physical properties for grade   KH20N80-VI   ( Х20Н80-ВИ )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20   12   8400    



Types of delivery of grade   KH20N80-VI   ( Х20Н80-ВИ )
B73 - Steel Alloy Wire


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  KH20N80-VI   ( Х20Н80-ВИ ) - Precision alloy with higt electric resistance: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys