Chemical composition in % for grade   68А   ( 68А )
C Si Mn Ni S P CrAl Cu
0.65 - 0.70.15 - 0.250.4 - 0.55max   0.2max   0.025max   0.025max   0.12max   0.05max   0.15


Equivalent steels for grade     68А   ( 68А )
Warning! Indicated both exact and nearest equivalents.
USAGermanyEnglandPolandAustralia
-DIN,WNrBSPNAS
G10650
K07001
C65S1
060A96
090A65
DS65G
1065

Types of delivery of grade   68А   ( 68А )
В72 - Medium-high and high-carbon steel wire


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  68А   ( 68А ) - Spring structural steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru