Characteristics for grade     10KH2M   ( 10Х2М )

      Grade :   10KH2M   ( 10Х2М ) (   10Х2М-ВД   )
      Classification :   Alloy structurall steel
      Equivalent grades:   Go here



Chemical composition in % for grade   10KH2M   ( 10Х2М )
C Si Mn Ni S P Cr Mo
0.08 - 0.120.17 - 0.370.4 - 0.7max   0.3max   0.02max   0.022 - 2.50.6 - 0.8


Mechanical properties under Т=20oС for grade   10KH2M   ( 10Х2М )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet, GOST 5520-79     390-590295 20  980 


Equivalent steels for grade     10KH2M   ( 10Х2М )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySwedenBulgariaHungaryPolandRomaniaCzechia
-DIN,WNrJIS AFNORBSEN UNISSBDSMSZPNSTASCSN
F22
10CrMo9-10
GS-12CrMo9-10
SFVAF22A
10CD9-10
11CrMo9-10
622-490
1.7380
10CrMo9-10
12CrMo9-10
2218
12Ch2M
2Cr10Mo45.47
10H2M
10CrMo10
12MoCr22
15313

Types of delivery of grade   10KH2M   ( 10Х2М )
B23 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  10KH2M   ( 10Х2М ) - Alloy structurall steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)