Chemical composition in % for grade   15KH18SYU   ( 15Х18СЮ )
C Si Mn S P CrAl
max   0.151 - 1.5max   0.8max   0.025max   0.03517 - 200.7 - 1.2


Mechanical properties under Т=20oС for grade   15KH18SYU   ( 15Х18СЮ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 5949-75     490 295 20 50 Annealing


Equivalent steels for grade     15KH18SYU   ( 15Х18СЮ )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySpainChinaBulgariaHungaryPolandRomaniaSouth Korea
-DIN,WNrJIS AFNORBSEN UNIUNEGBBDSMSZPNSTASKS
430
1.4742
X10CrAl18
X10CrAlSi18
SUN21
Z10CAS18
Z12CAS18
430S15
X10CrAlSi18
1.4742
X10CrAlSi18
X8Cr17
F.3113
F.3153
X10CrAl18
X10CrAlSi18
1Cr19Al3
Ch18SJu
H13
H18JS
10AlCr180
STR21


Assortment for grade   15KH18SYU   ( 15Х18СЮ )
В22 - Graded and shaped rolling
  GOST   1133 - 71 Forged round and square steel
  GOST   2590 - 2006 Steel hot-rolled round bars
  GOST   2591 - 2006 Steel hot-rolled square bars
  GOST   2879 - 2006 Hot-rolled hexagonal steel
B23 - Sheets and Strips
  GOST   103 - 2006 Hot-rolled steel strip
В32 - Graded and shaped rolling
  GOST   5949 - 75 Sorted and gauged corrosion-resistant, heat-resistant and high-temperature steel
  GOST   7417 - 75 Calibrated round steel
  GOST   8559 - 75 Calibrated square steel
B33 - Sheets and Strips
  GOST   4405 - 75 Hot-rolled and wrought tool steel strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

  15KH18SYU   ( 15Х18СЮ ) - High alloy high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru