Characteristics for grade     10KH13SYU   ( 10Х13СЮ )

      Grade :   10KH13SYU   ( 10Х13СЮ ) (   1Х12СЮ     ЭИ404   )
      Classification :   High alloy high-temperature steel
      Equivalent grades:   Go here
Grade   10KH13SYU   ( 10Х13СЮ ):   supplier   Auremo   www.auremo.biz
Sale:   Russia +7 (812) 680-16-77 ,   Germany +49 (208) 205-83-073,     info [a] auremo.org



Chemical composition in % for grade   10KH13SYU   ( 10Х13СЮ )
C Si Mn S P CrAl
0.07 - 0.121.2 - 2max   0.8max   0.025max   0.0312 - 141 - 1.8


Mechanical properties under Т=20oС for grade   10KH13SYU   ( 10Х13СЮ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 5949-75     490 345 15 60 Annealing 800 - 850oC, air,


Equivalent steels for grade     10KH13SYU   ( 10Х13СЮ )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySpainChinaBulgariaHungaryPolandCzechia
-DIN,WNrJIS AFNORBSEN UNIUNEGBBDSMSZPNCSN
405
MT405
S40500
1.4724
X10CrAl13
X7CrAl13
Х10CrAlSi13
SUS405
Z10C13
Z13C13
403S17
X10CrAlSi13
1.4724
X10CrAl13
X10CrAlSi13
X10CrSiAl13
X10CrAl12
F.311
F.3152
X10CrAl13
X10CrAlSi13
OCr13Al
Ch13SJu
H12
H13JS
17125

Types of delivery of grade   10KH13SYU   ( 10Х13СЮ )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  10KH13SYU   ( 10Х13СЮ ) - High alloy high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru