Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  

    YOU HERE:   Steel and Alloy   ->   High-temperature or heat-resistant steel and alloy

Characteristics for grade     12KH8VF   ( 12Х8ВФ )

      Grade :   12KH8VF   ( 12Х8ВФ ) (   1Х8ВФ   )
      Classification :   High alloy high-temperature steel
      Equivalent grades:     Is absent



Chemical composition in % for grade   12KH8VF   ( 12Х8ВФ )
C Si Mn Ni S P Cr W V
0.08 - 0.15max   0.6max   0.5max   0.6max   0.025max   0.037 - 8.50.6 - 10.3 - 0.5


Mechanical properties under Т=20oС for grade   12KH8VF   ( 12Х8ВФ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe hot strain, GOST 550-75     392 167 22 50980 
Bar, GOST 20072-74     390 165 22 50980Annealing 840 - 860oC, oven,


    Brinell hardness for     12KH8VF   ( 12Х8ВФ )   (hot-rolled, annealing) ,       GOST 20072-74 HB 10 -1 = 217   MPa
    Brinell hardness for     12KH8VF   ( 12Х8ВФ )   ,     Pipe GOST 550-75 HB 10 -1 = 170   MPa


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

  12KH8VF   ( 12Х8ВФ ) - High alloy high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru