Characteristics for grade     45KH14N14V2M   ( 45Х14Н14В2М )

      Grade :     45KH14N14V2M   ( 45Х14Н14В2М )
      Classification :   High alloy high-temperature steel
      Equivalent grades:   Go here



Chemical composition in % for grade   45KH14N14V2M   ( 45Х14Н14В2М )
C Si Mn Ni S P Cr Mo W
0.4 - 0.5max   0.8max   0.713 - 15max   0.02max   0.03513 - 150.25 - 0.42 - 2.8


Mechanical properties under Т=20oС for grade   45KH14N14V2M   ( 45Х14Н14В2М )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 5949-75     710 315 20 35 Drawing 810 - 830oC, air,


    Brinell hardness for     45KH14N14V2M   ( 45Х14Н14В2М )   (annealing) ,     Bar GOST 5949-75 HB 10 -1 = 197 - 285   MPa


Technological properties for grade   45KH14N14V2M   ( 45Х14Н14В2М )
  Weldability: hard weldability.


Physical properties for grade   45KH14N14V2M   ( 45Х14Н14В2М )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.08   14 8000   815
100 1.96   16     875
200 1.9 17 17 7930   945
300 1.81   19   507 1000
400 1.73 18 20 7840 511 1055
500 1.66   21   523 1098
600 1.57 18 22 7760 528 1142
700 1.49   24     1172
800 1.41 19   7660    
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     45KH14N14V2M   ( 45Х14Н14В2М )
Warning! Indicated both exact and nearest equivalents.
USAJapanFranceEnglandHungaryPolandCzechia
-JIS AFNORBSMSZPNCSN
S66009
SUH31
Z35CNWS14-14
331S42
SZ8
4H14N14W2M
17322


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  45KH14N14V2M   ( 45Х14Н14В2М ) - High alloy high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru