Characteristics for grade     10KH11N23T3MR   ( 10Х11Н23Т3МР )

      Grade :   10KH11N23T3MR   ( 10Х11Н23Т3МР ) (   Х12Н22Т3МР     ЭП33   )
      Classification :   High alloy high-temperature steel
      Equivalent grades:     Is absent



Chemical composition in % for grade   10KH11N23T3MR   ( 10Х11Н23Т3МР )
C Si Mn Ni S P Cr Mo TiAl B
max   0.1max   0.6max   0.621 - 25max   0.01max   0.02510 - 12.51 - 1.62.6 - 3.2max   0.8max   0.02


Mechanical properties under Т=20oС for grade   10KH11N23T3MR   ( 10Х11Н23Т3МР )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 5949-75     880-980590-6858-1010-12290Hardening and ageing


Assortment for grade   10KH11N23T3MR   ( 10Х11Н23Т3МР )
В22 - Graded and shaped rolling
  GOST   1133 - 71 Forged round and square steel
  GOST   2590 - 2006 Steel hot-rolled round bars
  GOST   2591 - 2006 Steel hot-rolled square bars
  GOST   2879 - 2006 Hot-rolled hexagonal steel
B23 - Sheets and Strips
  GOST   103 - 2006 Hot-rolled steel strip
В32 - Graded and shaped rolling
  GOST   8559 - 75 Calibrated square steel
  GOST   7417 - 75 Calibrated round steel
  GOST   5949 - 75 Sorted and gauged corrosion-resistant, heat-resistant and high-temperature steel
  GOST   8560 - 78 Steel calibrated, hexahedronal
B33 - Sheets and Strips
  GOST   4405 - 75 Hot-rolled and wrought tool steel strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

  10KH11N23T3MR   ( 10Х11Н23Т3МР ) - High alloy high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru