Characteristics for grade     13KH14N3V2FR   ( 13Х14Н3В2ФР )

      Grade :   13KH14N3V2FR   ( 13Х14Н3В2ФР ) (   Х14НВФР     ЭИ736   )
      Classification :   High alloy high-temperature steel
      Equivalent grades:     Is absent



Chemical composition in % for grade   13KH14N3V2FR   ( 13Х14Н3В2ФР )
C Si Mn Ni S P Cr W V Ti B
0.1 - 0.16max   0.6max   0.62.8 - 3.4max   0.025max   0.0313 - 151.6 - 2.20.18 - 0.28max   0.05max   0.004


Mechanical properties under Т=20oС for grade   13KH14N3V2FR   ( 13Х14Н3В2ФР )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 5949-75 to Ø 60   930 735 14 55880Guenching 1040 - 1060oC, oil, Drawing 640 - 680oC, air,
Bar, GOST 5949-75     1130 885 12 50690Guenching 1040 - 1060oC, air, Drawing 540 - 580oC, air,


    Brinell hardness for     13KH14N3V2FR   ( 13Х14Н3В2ФР )   (annealing) ,     Bar GOST 5949-75 HB 10 -1 = 302   MPa


Assortment for grade   13KH14N3V2FR   ( 13Х14Н3В2ФР )
В22 - Graded and shaped rolling
  GOST   2879 - 2006 Hot-rolled hexagonal steel
  GOST   1133 - 71 Forged round and square steel
  GOST   2590 - 2006 Steel hot-rolled round bars
  GOST   2591 - 2006 Steel hot-rolled square bars
B23 - Sheets and Strips
  GOST   103 - 2006 Hot-rolled steel strip
В32 - Graded and shaped rolling
  GOST   14955 - 77 Quality round steel with special surface finish
  GOST   5949 - 75 Sorted and gauged corrosion-resistant, heat-resistant and high-temperature steel
  GOST   7417 - 75 Calibrated round steel
  GOST   8559 - 75 Calibrated square steel
B33 - Sheets and Strips
  GOST   4405 - 75 Hot-rolled and wrought tool steel strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

  13KH14N3V2FR   ( 13Х14Н3В2ФР ) - High alloy high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru