Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Structural steel

Characteristics for grade     15   ( 15 )

      Grade :     15   ( 15 )
      Substitute:   10, 20
      Classification :   High quality structural carbon steel
      Equivalent grades:   Go here



Chemical composition in % for grade   15   ( 15 )
C Si Mn Ni S P Cr Cu As
0.12 - 0.190.17 - 0.370.35 - 0.65max   0.3max   0.04max   0.035max   0.25max   0.3max   0.08


Temperature of critical points for grade   15   ( 15 ).
Ac1 = 735 ,      Ac3(Acm) = 860 ,       Ar3(Arcm) = 840 ,       Ar1 = 685


Mechanical properties under Т=20oС for grade   15   ( 15 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet heat-treatment, GOST 4041-71 4 - 14   320-440  30    
Pipe, GOST 5005-82     510 430 8    
Rolled stock, GOST 1050-88 to 80   370 225 27 55 Normalizing
Rolled stock cold-worked , GOST 1050-88     440   8 45  
Rolled stock annealed , GOST 1050-88     340   23 55  
Band annealed , GOST 2284-79     310-490  20    
Band cold-worked , GOST 2284-79     440-780       


    Brinell hardness for     15   ( 15 )   ,     Sheet GOST 4041-71 HB 10 -1 = 121   MPa
    Brinell hardness for     15   ( 15 )   ,     Bar GOST 10702-78 HB 10 -1 = 125   MPa
    Brinell hardness for     15   ( 15 )   ,     Rolled stock GOST 1050-88 HB 10 -1 = 197   MPa
    Brinell hardness for     15   ( 15 )   ,     Rolled stock GOST 1050-88 HB 10 -1 = 149   MPa
    Brinell hardness for     15   ( 15 )   ,     Rolled stock GOST 1050-88 HB 10 -1 = 149   MPa
    Brinell hardness for     15   ( 15 )   ,     Sheet trick GOST 1577-93 HB 10 -1 = 143   MPa


Technological properties for grade   15   ( 15 )
  Weldability: without limitations.
 Flakes : not predisposed
Temper brittleness: not predisposed


Physical properties for grade   15   ( 15 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.01   53 7850    
100 1.92 12.4 53 7827 465 233
200 1.85 13.2 53 7794 486 296
300 1.76 13.9 49 7759 515 387
400 1.56 14.4 46 7724 532 487
500   14.8 43 7687 565 607
600   15.1 39 7648 586 753
700   15.3 36 7611 620 904
800   14.1 32 7599 691 1092
900   13.2 30 7584 708 1140
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     15   ( 15 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalyBelgiumSpainChinaSwedenBulgariaHungaryPolandRomaniaCzechiaAustriaSwitzerlandSouth Korea
-DIN,WNrJIS AFNORBSEN UNINBNUNEGBSSBDSMSZPNSTASCSNONORMSNVKS
1015
1016
1017
1018
G10150
G10170
M1015
M1017
1.0401
1.1141
C15
C15E
Ck15
Cq15
RSt42-2
S15
S15C
S15CK
S17C
C18RR
XC12
XC15
XC18
040A15
080M15
C15E
1.1132
1.1141
2C15
C15E2C
C15Е
C15
C16
C16-2
C15E
C15k
C16k
F.1110
F.1511
15
H15A
ZG200-400
1370
15
C15
15
OLC15
OLC15AT
OLC15X
12020
12023
RC15
Ck15
SM15C
SM15CK

Types of delivery of grade   15   ( 15 )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
B24 - Ribbons
В32 - Graded and shaped rolling
B33 - Sheets and Strips
B34 - Ribbons
В62 - Steel pipes and connecting parts to them
В71 - Low-carbon steel wire
В72 - Medium-high and high-carbon steel wire
B76 - Metal nets


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  15   ( 15 ) - High quality structural carbon steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru