Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | S-NiSiCr20-5-2 ( S-NiSiCr20-5-2 ) |
Classification : | Nickel cast iron |
Equivalent grades: | Is absent |
C | Si | Mn | Ni | P | Cr | Cu |
max 3 | 4.5 - 5.5 | 0.5 - 1.5 | 18 - 22 | max 0.08 | 1 - 2.5 | max 0.5 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Casting, GOST 7769-82 | 370-430 | 210-260 | 14 |
Brinell hardness for S-NiSiCr20-5-2 ( S-NiSiCr20-5-2 ) , GOST 7769-82 | HB 10 -1 = 180 - 230 MPa |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 1.22 |
В81 - Castings of cast iron (gray and malleable cast iron) |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |