Characteristics for grade     08YU   ( 08Ю )

      Grade :     08YU   ( 08Ю )
      Classification :   High quality structural carbon steel
      Equivalent grades:   Go here



Chemical composition in % for grade   08YU   ( 08Ю )
C Si Mn S PAl
max   0.07max   0.03max   0.35max   0.025max   0.020.02 - 0.07


Mechanical properties under Т=20oС for grade   08YU   ( 08Ю )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet heat-treatment, GOST 4041-71 4 - 8   360   36    
Pipe, GOST 10705-80     255 174 30    
Strip, GOST 1577-93 6 - 60   290 175 35 60 Normalizing


    Brinell hardness for     08YU   ( 08Ю )   ,     Sheet GOST 4041-71 HB 10 -1 = 118   MPa
    Brinell hardness for     08YU   ( 08Ю )   (annealing) ,     Strip GOST 1577-93 HB 10 -1 = 131   MPa


Technological properties for grade   08YU   ( 08Ю )
  Weldability: without limitations.
 Flakes : not predisposed
Temper brittleness: not predisposed


Equivalent steels for grade     08YU   ( 08Ю )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySpainSwedenPolandRomaniaCzechiaFinlandAustriaAustralia
-DIN,WNrJIS AFNORBSEN UNIUNESSPNSTASCSNSFSONORMAS
A619
A620
K00040
1.0338
1.0346
1.0347
DC03
DC04
DC04G1
RRSt3
St12
St14
St4
CR4
SPCC
SPCE
3C
DC03
E
ES
FeP01
1449-12CR
1449-1CR
1449-3CR
1CS
1HR
1HS
2HR
3HR
DC03
DC04
FeP01
1.0330
1.0347
DC01
DC03
E
FeP03
FeP04
DC01
DC03
DC04
FeP02
FeP04
AP04
DC03
DC04
1142
1147
08J
08JA
A3k
11305
11321
RACOLD03F
RACOLD04F
St02F
St04F
CA2
CA3
CA4
HA3
HA4N

Types of delivery of grade   08YU   ( 08Ю )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
B33 - Sheets and Strips
B34 - Ribbons
В62 - Steel pipes and connecting parts to them


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  08YU   ( 08Ю ) - High quality structural carbon steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru