Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | 3405 ( 3405 ) |
Classification : | Electrotechnical sulphide steel |
Equivalent grades: | Is absent |
Si | - |
2.8 - 3.8 | Chemical composition is not regimented |
Assortment | Dimension | Hc | μmax | P1.0/50 | P1.5/50 | B100 | B500 | B1000 | B2500 | B5000 | B10000 | B30000 |
- | mm | A/m | - | W/kg | W/kg | A/m | A/m | A/m | A/m | A/m | A/m | A/m |
Sheet cold-rolled | 0.35 | 1.61 |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 7650 | 500 |
B33 - Sheets and Strips |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
Magnetic properties : | |
Hc | - Coercive force [ A/m ] |
μmax | - Magnetic permeability [ ] |
P1.0/50 | - Maximum specific total loss at [ W/kg ] |
B100 | - Minimum magnetic flux density T for H, [ А/m ] |