Characteristics for grade     16k   ( 16К )

      Grade :     16k   ( 16К )
      Classification :   High quality structural carbon steel
      Equivalent grades:   Go here



Chemical composition in % for grade   16k   ( 16К )
C Si Mn Ni S P Cr Cu As
0.12 - 0.20.17 - 0.370.45 - 0.75max   0.3max   0.04max   0.04max   0.3max   0.3max   0.08


Mechanical properties under Т=20oС for grade   16k   ( 16К )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet, GOST 5520-79     400-490235-25522  690 


Technological properties for grade   16k   ( 16К )
  Weldability: without limitations.


Equivalent steels for grade     16k   ( 16К )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalyBelgiumSpainSwedenBulgariaHungaryPolandRomaniaCzechiaAustriaSouth Korea
-DIN,WNrJIS AFNORBSEN UNINBNUNESSBDSMSZPNSTASCSNONORMKS
Gr.A
K01701
K02100
K02401
K02402
K02505
1.0425
C22N
H2
HII
P269GH
SG295
SG30
SGV410
SGV450
SGV480
SPV235
SPV315
SPV355
A42AP
A42CP
P265GH
1501Gr.161-400
151-400
154-400
161-400
P269GH
1.0425
P269GH
Fe4101KG
Fe4101KT
Fe4101KW
Fe410KG
Fe410KT
Fe410KW
P269GH
D42-1
A42RCI
A42RCII
1430
1431
1432
16K
P265GH
KL2
KL2C
P265GH
St41K
K410
OL44.3
11416
St41KW
SPPV315
SPPV355

Types of delivery of grade   16k   ( 16К )
B23 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  16k   ( 16К ) - High quality structural carbon steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru