Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   High-temperature or heat-resistant steel and alloy

Characteristics for grade     KhN70MVTYuB   ( ХН70МВТЮБ )

      Grade :   KhN70MVTYuB   ( ХН70МВТЮБ ) (   ЭИ598     ХН70МВТЮБ-ВИ     ЭИ598-ВИ     ХН70МВТЮБ-ВД     ЭИ598-ВД   )
      Classification :   Hidh-temperature or heat-resistant alloy
      Equivalent grades:     Is absent
Grade   KhN70MVTYuB   ( ХН70МВТЮБ ):   supplier   Auremo   www.auremo.biz
Sale:   Russia +7 (812) 680-16-77 ,   Germany +49 (208) 205-83-073,     info [a] auremo.org



Chemical composition in % for grade   KhN70MVTYuB   ( ХН70МВТЮБ )
Fe C Si Mn Ni S P Cr Ce Mo W Nb TiAl B
max   5max   0.12max   0.6max   0.559.425 - 74.6max   0.01max   0.01516 - 19max   0.024 - 62 - 3.50.5 - 1.31.9 - 2.81 - 1.7max   0.01
Comment: Ni is a basis; the percentage of Ni is given approximately.


Mechanical properties under Т=20oС for grade   KhN70MVTYuB   ( ХН70МВТЮБ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 23705-79     690   6-1010-14 Hardening and ageing


    Brinell hardness for     KhN70MVTYuB   ( ХН70МВТЮБ )   (quenching, ageing) ,     Bar GOST 23705-79 HB 10 -1 = 299 - 341   MPa

Types of delivery of grade   KhN70MVTYuB   ( ХН70МВТЮБ )
В32 - Graded and shaped rolling


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  KhN70MVTYuB   ( ХН70МВТЮБ ) - Hidh-temperature or heat-resistant alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru