Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  

    YOU HERE:   Steel and Alloy   ->   High-temperature or heat-resistant steel and alloy

Characteristics for grade     KhN75VMYu   ( ХН75ВМЮ )

      Grade :   KhN75VMYu   ( ХН75ВМЮ ) (   ЭИ827   )
      Classification :   Hidh-temperature or heat-resistant alloy
      Equivalent grades:     Is absent



Chemical composition in % for grade   KhN75VMYu   ( ХН75ВМЮ )
Fe C Si Mn Ni S P Cr Ce Mo W VAl B
max   5max   0.12max   0.4max   0.465.725 - 77.49max   0.01max   0.0159 - 11max   0.015 - 6.54.5 - 5.5max   0.74 - 4.60.01 - 0.02
Comment: Ni is a basis; the percentage of Ni is given approximately.


Mechanical properties under Т=20oС for grade   KhN75VMYu   ( ХН75ВМЮ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 23705-79     590   6 9 Hardening and ageing


    Brinell hardness for     KhN75VMYu   ( ХН75ВМЮ )   ,     Bar GOST 23705-79 HB 10 -1 = 255 - 321   MPa


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

  KhN75VMYu   ( ХН75ВМЮ ) - Hidh-temperature or heat-resistant alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru