Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | 50NKHS ( 50НХС ) |
Classification : | Magnetically soft precision alloy |
Equivalent grades: | Is absent |
Fe | C | Si | Mn | Ni | S | P | Cr | Cu |
42.03 - 45 | max 0.03 | 1.1 - 1.4 | 0.6 - 1.1 | 49.5 - 51 | max 0.02 | max 0.02 | 3.8 - 4.2 | max 0.2 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Band, GOST 10160-75 | 490 | 145 | 40 | |||||
Band cold-worked , GOST 10160-75 | 880 | 835 | 2 |
Brinell hardness for 50NKHS ( 50НХС ) , Band GOST 10160-75 | HB 10 -1 = 125 MPa |
Brinell hardness for 50NKHS ( 50НХС ) , Band GOST 10160-75 | HB 10 -1 = 190 MPa |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 2.1 | 8200 | 900 |
В30 - Classification, nomenclature and general norms |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2025 Database of Steel and Alloy (russian title is the Marochnik)