Characteristics for grade     20KH12N2V2MF   ( 20Х12Н2В2МФ )

      Grade :     20KH12N2V2MF   ( 20Х12Н2В2МФ )
      Classification :   High alloy high-temperature steel
      Equivalent grades:     Is absent



Chemical composition in % for grade   20KH12N2V2MF   ( 20Х12Н2В2МФ )
C Si Mn Ni S P Cr Mo W V
0.09 - 0.13max   0.6max   0.61.5 - 1.8max   0.025max   0.0310.5 - 120.35 - 0.51.6 - 20.18 - 0.3


Mechanical properties under Т=20oС for grade   20KH12N2V2MF   ( 20Х12Н2В2МФ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet 0.8 - 4   650 450 19   Drawing 730 - 750oC, 2h,Cooling air,


Technological properties for grade   20KH12N2V2MF   ( 20Х12Н2В2МФ )
  Weldability: without limitations.


Physical properties for grade   20KH12N2V2MF   ( 20Х12Н2В2МФ )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2   20.9 7800    
100 1.95 11 22.3      
200 1.85 11.7 24      
300 1.75 12.2 25.5      
400 1.65 13.3 27.2      
500 1.45 13 28      
600 1.09 13 28.5      
T E 10- 5 a 10 6 l r C R 10 9


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  20KH12N2V2MF   ( 20Х12Н2В2МФ ) - High alloy high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru