Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   High-temperature or heat-resistant steel and alloy

Characteristics for grade     10KH15N25M3V3TYUK   ( 10Х15Н25М3В3ТЮК )

      Grade :     10KH15N25M3V3TYUK   ( 10Х15Н25М3В3ТЮК )
      Classification :   High alloy high-temperature steel
      Equivalent grades:     Is absent
Grade   10KH15N25M3V3TYUK   ( 10Х15Н25М3В3ТЮК ):   supplier   Auremo   www.auremo.biz
Sale:   Russia +7 (812) 680-16-77 ,   Germany +49 (208) 205-83-073,     info [a] auremo.org



Chemical composition in % for grade   10KH15N25M3V3TYUK   ( 10Х15Н25М3В3ТЮК )
Fe C Si Mn Ni S P Cr Mo W Co TiAl B
43.75 - 54.8max   0.1max   0.51 - 224 - 28max   0.02max   0.0214 - 162 - 32 - 30.5 - 10.9 - 1.30.8 - 1.3max   0.01


Mechanical properties under Т=20oС for grade   10KH15N25M3V3TYUK   ( 10Х15Н25М3В3ТЮК )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Strip   longitudinal 890 420 33 471400Guenching 1080 - 1100oC, water, Ageing Cooling air,


    Brinell hardness for     10KH15N25M3V3TYUK   ( 10Х15Н25М3В3ТЮК )   ,       HB 10 -1 = 228   MPa


Physical properties for grade   10KH15N25M3V3TYUK   ( 10Х15Н25М3В3ТЮК )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.02     8160    
100 1.99 14.5        
200 1.94 15.8        
300 1.9 16.1        
400 1.83 16.2        
500 1.77 16.8        
600 1.69 17.1        
700 1.61 17.4        
800 1.53          
T E 10- 5 a 10 6 l r C R 10 9


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  10KH15N25M3V3TYUK   ( 10Х15Н25М3В3ТЮК ) - High alloy high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com