Country - England | Standard - BS | Grade - LM9 |
AK9ch ( АК9ч ) - Aluminium casting alloys АK9 ( АК9 ) - Aluminium casting alloys AK9ch ( АК9ч ), АK9 ( АК9 ), |
B51 - Non-ferrous metals, including rare metals, and their alloys |
B51 - Non-ferrous metals, including rare metals, and their alloys |