Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Country - Japan | Standard - JIS G4104 | Grade - SCr435 |
35KH ( 35Х ) - Alloy structurall steel 40KH ( 40Х ) - Alloy structurall steel 38KHА ( 38ХА ) - Alloy structurall steel 35KH ( 35Х ), 40KH ( 40Х ), 38KHА ( 38ХА ), |
B03 - Metal forming treatment. Forgings |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
В71 - Low-carbon steel wire |
B03 - Metal forming treatment. Forgings |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
В62 - Steel pipes and connecting parts to them |
В71 - Low-carbon steel wire |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
В62 - Steel pipes and connecting parts to them |
В71 - Low-carbon steel wire |
© 2003 - 2024 Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use. |